Successful Testing by Certified Independent Labs includes the following:
- ASTM 1018, Static Flexural Strength
- ASTM C 173, Air Content and Unit Wt.
- ASTM C 39, Compressive Strength
- ASTM C 78, Flexural Strength
- ICC AC217-Annex A, Evaluating Plastic Shrinkage Cracking
- ASTM C 666(A), Freeze Thaw
- ASTM C 234, Bond Strength
- ASTM D 6942, Alkaline Stability
- ICC AC217-Annex B, Evaluating Impact Resistance
- ASTM C 856, Hydration
- ASTM C 1399, Average Residual Strength
- ISO 834, Fire Resistance
- AC1544, Impact Resistance
Specifications
- Avg. Fiber Length 2.1mm
- Avg. Denier 2.5
- Avg. Fiber Diameter 18 microns
- Fiber Count 720,000,000 fibers/lb
- Fiber Density 1.1 g/cm3
- Fiber Surface Area 25,000 cm2/g
- Avg. Fiber Tensile 110 KSI
Patent Granted and Patents Pending
In concrete at 1.5 lb/cy dosage:
- Fiber Count 1,080,000,000 fibers/cy
- Fiber Spacing 640 microns
|
 |

Concrete cylinder testing for
UltraFiber 500™ compressive strength
|